tuta

Busasshen Fim mai Inganci - Busashen Fim ɗin da Aka Aiwatar Akan FPC Da PCB - Mai Sa'a Innovative

Busasshen Fim mai Inganci - Busashen Fim ɗin da Aka Aiwatar Akan FPC Da PCB - Mai Sa'a Innovative

Takaitaccen Bayani:


Cikakken Bayani

Tags samfurin

Bidiyo mai alaka

Jawabin (2)

Wannan yana da ingantacciyar hali da ci gaba ga sha'awar abokin ciniki, ƙungiyarmu koyaushe tana haɓaka ingancin samfuranmu don biyan buƙatun masu siyayya da ƙara mai da hankali kan aminci, aminci, ƙayyadaddun muhalli, da sabbin abubuwaSaka Fim ɗin Molding Technologies,Hico Stripe,Yadda Ake Gwaji Gasken Kai, Muna sa ran yin hadin gwiwa tare da ku bisa tushen samun moriyar juna da ci gaba tare. Ba za mu taba ba ku kunya ba.
Busasshen Fim mai Inganci - Busashen Fim ɗin da Aka Aiwatar Akan FPC Da PCB - Cikakken Cikakkun Sabunta:

Aikace-aikacen samfur

Aiwatar da Hukumar da'ira da Bugawa da Hukumar da'ira mai sassauƙa, tare da fa'idar kyakkyawan aiki na kulawa, ƙuduri da mannewa.

Tsarin Samfur

Bushewar fim

Ƙayyadaddun samfur

Lambar samfur

LK-D1238 LDI Dry Film

LK-G1038 Dry Film

Kauri (μm)

38.0± 2.0

Tsawon (m)

200 m

Nisa

Bisa ga bukatar abokan ciniki

Sigar Samfura

(1) LK-D1238 LDI Dry Film

LK-D1238 LDI Dry Film ya dace da na'ura mai ɗaukar hoto kai tsaye, tare da tsawon tsayin 355nm da 405nm.

Abu da Hanyar Gwaji

Gwaji Data

Mafi qarancin lokacin hoto

(1.0wt.% Maganin ruwa Na2CO3, 30℃) *2

25s ku

Tsawon tsayi (nm)

355

405

Ayyuka bayan Hoto

Hankalin hoto

(*2×2.0)

ST=7/21

Fitar kuzari*3

20mJ/cm2

15mJ/cm2

Ƙimar (*2×2.0)

ST=6/21

40 μm

40 μm

ST=7/21

40 μm

40 μm

ST=8/21

50 μm

50 μm

Adhesion (*2×2.0)

ST=6/21

50 μm

50 μm

ST=7/21

40 μm

40 μm

ST=8/21

35m ku

35m ku

【Tasirin Amincewa】*3

10 ramuka (6mmφ)

Yawan karya rami

(*2×2.0×3 sau)

ST=6/21

0%

0%

ST=7/21

0%

0%

ST=8/21

0%

0%

Lokacin ƙarshen tsiri

(3.0wt.% Maganin ruwa na NaOH, 50℃)

ST=7/21* 1

Fitar kuzari

50s

50s

 

(2) LK-G1038 Dry Film

LK-G1038 Dry Film ya dace don tuntuɓar na'ura mai ɗaukar hoto, tare da babban tsawon 365nm.

Abu da Hanyar Gwaji

Gwaji Data

Mafi qarancin lokacin hoto

(1.0wt.% Maganin ruwa Na2CO3, 30℃) *2

22s

Ayyuka bayan Hoto

Hankalin hoto

(*2×2.0)

ST=8/21

Fitar kuzari*3

90mJ/cm2

Ƙaddamarwa

(*2×2.0)

ST=6/21

32.5m ku

ST=7/21*1

32.5m ku

ST=8/21

35m ku

Adhesion

(*2×2.0)

ST=6/21

45m ku

ST=7/21

40 μm

ST=8/21

35m ku

(Tsarin Amincewa)*3

10 ramuka (6mmφ)

Yawan karya rami

(*2×2.0×3 sau)

ST=6/21

0%

ST=7/21

0%

ST=8/21

0%

Lokacin ƙarshen tsiri

(3.0wt.% Maganin NaOHwater, 50℃)

ST=7/21*1

Fitar kuzari

50s

(Bayanan da ke sama don tunani ne kawai)
Lura:

*1: Stouffer 21 Matsayin Fuskar Makamashi.
* 2 × 2.0: Hoto tare da sau biyu mafi ƙarancin lokacin hoto.
*3: Idan mai da hankali kan Amintaccen Tending, ana ba da shawarar yin amfani da ƙimar kuzarin fallasa matakin 7 ~ 8.
*4: Abubuwan da ke sama ana gwada su ta kayan aikin mu da kayan aikin mu.

Tsarin Aikace-aikacen

samfur

Tsanaki A Aikace-aikace

(1) Aikace-aikace : Yi amfani da wannan fim ɗin kawai azaman tsayayya don abubuwan da ke da alaƙa da allon da'ira da sauran ƙirar ƙira.
(2) Pretreatment : Organic sharan gona, stains saboda kasa dewatering da bushewa a kan jan karfe surface, na iya haifar da polymerization na juriya da shigar da plating ko etching bayani.Don Allah bushe gaba daya bayan ruwa rinsing. Musamman, lokacin da danshi ya kasance a cikin ramin, yana haifar da karyewar tanti.
(3) Substrate preheating : Preheating a ma high zafin jiki na dogon lokaci na iya haifar da tsatsa.Ya kamata a yi kasa da 10 min a 80 ℃ da kasa da 3 min a 150 ℃. Kuma lokacin da zafin jiki na saman ƙasa kafin lamination ya wuce 70 ℃, kauri na fim ɗin akan gefen rami na iya zama bakin ciki sosai kuma yana iya haifar da fashewar tent.
(4) Rike bayan lamination da fallasa: Rike da garkuwar haske ko ƙarƙashin fitilar rawaya (mita 2 ko fiye da nisa da ake buƙata). Matsakaicin lokacin riƙewa a cikin akwati na ƙarshe (ƙarƙashin fitilar rawaya) kwanaki 4 ne. Ya kamata a yi nuni a cikin kwanaki 4 bayan lamination. Ya kamata a yi ci gaba a cikin kwanaki 3 bayan bayyanarwa. Ray of non-ultraviolet farin fitila yana da wasu ultraviolet haskoki, don haka rike da haske garkuwa ta baƙar fata sheet a ƙarƙashinsa.Keep zazzabi 23±2℃ da dangi zafi 60±10% RH. Ya kamata a saka kayan da aka lakafta a cikin rakiyar daya bayan daya.
(5) Haɓakawa: Lokacin da zafin jiki na mai haɓakawa ya wuce 35 ℃, yana iya yin tsayayya da bayanin martaba mafi muni.
(6) Cire : Tafi cikin mako guda bayan lamination.
(7) Maganin sharar gida: Abubuwan da aka bushe na fim a cikin masu haɓakawa da kuma tsiri za a iya haɗa su ta hanyar neutralization. Za a iya raba abubuwan da aka haɗar da su daga maganin ruwa ta hanyar latsa tacewa da hanyar centrifugal. Maganin ruwan ruwa da aka ware yana da wasu ƙimar COD da BOD, don haka dole ne a bi da shi ta hanyar da ta dace.
(8) Launin fim : Kalar kore/ shuɗi ne. Kodayake launi na iya canzawa a hankali tare da lokaci, bai kamata ya rinjayi halayyar ba.

Tsanaki Kan Ajiya

(1) Lokacin da aka yi ajiya a cikin duhu, sanyi, da bushe wuri a zazzabi na 5 ℃ 20 ℃ da dangi zafi na 60% RH ko žasa, bushe fim ya kamata a yi amfani da a cikin kwanaki 50 bayan yi.
(2) Rike fim ɗin yana jujjuya shi a kwance ta hanyar amfani da racks ko allunan tallafi don ajiya. Lokacin da aka shimfiɗa su a tsaye, busassun fim ɗin za su iya zamewa ɗaya bayan ɗaya kuma siffar birgima na iya zama kamar tsiron bamboo (ana kwance a kwance a cikin kunshin).
(3) Cire nadi na fina-finai daga baƙar fata a ƙarƙashin fitilar rawaya ko nau'in fitilar aminci iri ɗaya. Kada ku bar su a ƙarƙashin fitilar rawaya na dogon lokaci. Rufe fim ɗin da baƙar fata lokacin da kuka adana su na dogon lokaci.


Hotuna dalla-dalla samfurin:

Busashen Fim mai Inganci - Busashen Fim ɗin da Aka Aiwatar Akan FPC Da PCB - Hoton daki-daki masu ban sha'awa

Busashen Fim mai Inganci - Busashen Fim ɗin da Aka Aiwatar Akan FPC Da PCB - Hoton daki-daki masu ban sha'awa

Busashen Fim mai Inganci - Busashen Fim ɗin da Aka Aiwatar Akan FPC Da PCB - Hoton daki-daki masu ban sha'awa

Busashen Fim mai Inganci - Busashen Fim ɗin da Aka Aiwatar Akan FPC Da PCB - Hoton daki-daki masu ban sha'awa

Busashen Fim mai Inganci - Busashen Fim ɗin da Aka Aiwatar Akan FPC Da PCB - Hoton daki-daki masu ban sha'awa


Jagoran Samfuri masu alaƙa:

Mun yanzu tabbas mafi m samar da kayan aiki, gogaggen da qualified injiniyoyi da ma'aikata, dauke high quality kula da tsarin da kuma abokantaka gwani samun kudin shiga tawagar pre / bayan-tallace-tallace goyon bayan Good Quality Dry Film - Dry Film Applied On FPC Kuma PCB - Lucky Innovative , The samfurin zai wadata ga ko'ina cikin duniya, kamar: Sudan , Maroko , Girka , Our abokin ciniki idanu sa mu muhimmanci a mu abokin ciniki. Our ingancin magana da kanta da kaddarorin kamar shi ba tangle, zubar ko rushewa, don haka su ne abokan cinikinmu koyaushe za su kasance masu ƙarfin gwiwa yayin yin oda.
  • Koyaushe muna yin imani cewa cikakkun bayanai sun yanke shawarar ingancin samfurin kamfanin, ta wannan yanayin, kamfanin yana biyan bukatunmu kuma kayayyaki sun cika tsammaninmu.
    Taurari 5By Miriam daga Frankfurt - 2018.09.12 17:18
    An yaba mana masana'antar Sinawa, wannan lokacin kuma bai bar mu mu yanke ƙauna ba, kyakkyawan aiki!
    Taurari 5By Alice daga Accra - 2017.09.16 13:44
    Ku rubuta sakonku anan ku aiko mana